Victor,
The short answer is no color change is expected but if the part is experiencing internal heating then all bets are off.
Regards,
John Maxwell
> On Aug 25, 2016, at 2:59 PM, Victor Hernandez <[log in to unmask]> wrote:
>
> Fellow TechNetters:
>
> During the service life of a ceramic capacitor will the ceramic material color change in color due to normal usage? How about if the circuit draws too much current, overheating condition/leakage.
>
> Victor,
|
|
|