I was considering the same situation a couple of years ago and asked the
same question in this forum. Essentially, the answers indicated that the
older, single-reflow OSPs have been used for years (10+) in many
applications with compliant pin connectors with no problems, but that there
was not much data on the thicker multiple-reflow OSPs (which was being used
for the applications I was considering). In the absence of this data, we
did our own testing (including shock/vibe, temp cycling, temp/humidity,
high temp tests) and found no problems. Similarly, there have been no
problems with this combination on live products since introduced a year or
two ago.
I'd echo the point about ensuring that the fixturing and backing plate
being sound before proceeding.
Regards,
Greg Bartlett
Teledyne Electronic Technologies
Hudson, NH
[log in to unmask]
-------
In a message dated 08/24/98 7:16:37 PM Pacific Daylight Time,
[log in to unmask]
writes:
> Will there be any problem if my board surface finish is OSP and has a
> press-fit connector?
>
> Re,
> Ken Patel
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|