Some people use RTV as the generic term for any silicone based adhesive.
Common RTV does out-gas causing corrision.
Try the following companies:
ABLESTIK ELECTRONIC: MATERIALS
20021 Susana Road
Rancho Dominguez, California 90221 U.S.A.
Phone (310) 764.4600
Fax 310.764.2545
ARLON INC.
Silicone Technologies Division
1100 Governor Lea Road Bear, Delaware 19701
Phone: 1-800-635-9333 Fax: 1-302-834-4021
General Electric Company
260 Hudson River Road
Waterford, NY 12188
Technical Assistance
800-255-8886
Customer Service
800-332-3390
3M Company
Industrial Materials
Department
3M Center
Saint Paul, MN 55144
Gen. Info: 800 364-3577
Tech Info: 612 736-0315
TRA-CON, Inc.
45 Wiggins Ave
Bedford, MA 01730 USA
tel: 781-275-6363
fax: 781-275-9249
There are many other companies, but I've only tested materials from these.
Mike
Research Assistant
CALCE/EPRC UMCP
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|