TECHNET Archives

January 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Date:
Fri, 19 Jan 2001 13:33:26 -0600
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
IPC 6012 is actually the 'controlling' document whereas A 600 is an
acceptance guideline 'after' the product has been fabricated. Basically
6012 states fabrication result criteria and A 600 provides visual
guidelines for the same.

Since IPC A 600 was introduced prior to 6012 (before 6012 there was RB
276, prior to that some ML number, and so on, and so on) I believe most
people believe that to be 'the' document to reference.

When a fabricator states on their documents they meet A 600 this can be
assumed they were 'inspected' in accordance with that document, and not
'fabricated' in accordance with that document.

We try to educate our customers when they submit procuement documents
stating 'fabricate and inspecto to...A 600'. We explain we will utilize
applicable elements of 6012 for fabrication

Hope this helps someone.

Franklin

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2