I have also used the Metcal 1XX tips. They worked quite well, and seemed
to last as long as regular tips in spite of the higher heat sometimes
needed. However, I found that we did not really have to increase the tip
temperature by more than 10-20 degrees or so to get identical wetting
with the SAC305 Kester alloy for water wash wire solder. There was not
any noticeable slowdown in the hand solder process. This was at a CEM
where I worked previously, and they stated that if anything, there has
been an improvement in time required to hand solder. I do recall that we
went to a higher percentage of flux content, I think from 1.5% to 2.5%
when we switched from 63/37 to SAC305. This may have helped.
I have no experience with the Pb-free no-clean wire solder, but based on
the 63/37 no-clean wire solder's tendency to burn of the plating on the
soldering iron tips much faster, I would expect difficulty when changing
over to a Pb-free no-clean.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Monday, August 08, 2005 10:24 PM
To: [log in to unmask]
Subject: Re: [TN] LeadFree Solder Iron
MetCal. Use the special higher temp tip. I think they are designated as
their "1XX" tips.
Rich K/ KEDS
________________________________
From: TechNet on behalf of Poh Kong Hui
Sent: Sun 8/7/2005 9:20 PM
To: [log in to unmask]
Subject: Re: [TN] LeadFree Solder Iron
Hi,
Can anyone who is doing lead free soldering, make recommendation of
which brand of solder iron you are using, which you find good.
I evaluate couple of brands, it seems none of them that I try seems OK.
The lead free soldering is difficult & slow as compared to tin-lead
solder.
In fact, every lead free processes need more heat energy.
Thanks.
KH Poh
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|