TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Steve Underwood <[log in to unmask]>
Date:
Sun, 13 Aug 2000 21:04:07 -0400
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Steve Underwood <[log in to unmask]>
Parts/Attachments:
text/plain (43 lines)
I sent this message to TechNet on 08/10/2000.
Did this message make it to the list?  I did not get any responses.

:-) I'm interested to know how y'all interpret IPC-2221,
:-) section 12.4.1 "Specimen A and B (Plated Hole Evaluation)..."
:-) "Spacing between holes shall be representative of the
:-) printed board.  Conductors shall be included in between the
:-) holes on each signal layer."
:-)
:-) I have the interpretation that the spacing between the
:-) holes (with the traces between them) will be determined by
:-) the worst case pad to trace spacing on the design.  So, if
:-) there are 6 mil lines and 6 mil spaces on the internal
:-) layers but only 8 mil lines and 8 mil spaces on the outer
:-) layers, I would have to set up the coupon with the 6 mil
:-) line and space throughout the entire coupon stack.  This
:-) seems to make the outer layer of the coupon then NOT match
:-) the outer layer of the board and the coupon may fail where
:-) the board may not.
:-)
:-) Do you make an extra set of A & B coupons for each
:-) different spacing configuration?
:-)
:-) Do you mix the hole to hole and pad to trace spacings on
:-) the coupons and potentially increase the size and/or
:-) complexity of the coupon?
:-)
:-) Steve

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2