We are using the wire insulated with high temp cloth, Kevlar I believe.
We have used them many times. The voltage / temperature values are
unchanged.
This is a fundamental property of the materials. I would not expect to see
subtle drifting.
If the weld is good and the connection at the plug is good, the wires
insulated one from the other up to the weld, the voltage measured at the
ends of the wire should be reliable and temperature dependent.
I have seen failures of the insulation, cracks in the weld, and loose
connections inside the plug produce inaccurate measurements.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 02, 2007 2:04 PM
To: [log in to unmask]
Subject: [TN] Thermocouple Longevity?
Hi Everyone!
How many reflow profiles do ya'll put the same thermocouples through before
you think about replacing them?
I've typically used them until they quit working or the insulation
deteriorates so bad that I don't want to use them anymore. I was told that
was not a good practice. That your typical K thermocouple starts drifting
after only 4 or 5 thermal cycles. I said; "Really?" I didn't want to debate
a whole lot because it was a customer who said this, so I just agreed and
went on.
So, do any of you know this to be a fact, and do any of you trash a
thermocouple after only 4 or 5 profiles and replace them with new ones?
Kind regards,
Steve Gregory
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|