Hi all,

For SMT double-sided boards we will typically solderpaste all vias on the bottom
side for vacuum test reasons.  For a single-sided SMT board, it makes sense to
do this on the top side (costly to create another stencil just to paste vias on
the bottom side).

My question is this....we have a prototype that has several vias located beneath
some pretty low profile TSOPs, where the body is 2-8 mils off the board.  I've
come to understand that a 6-8 mil solder print is typical.  Has anyone
experienced shorting of vias beneath low profile parts due to the paste?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2