Robert,
Surprising you have this problem in GI mat'l. Sure you do not have this in
GF mat'l ?. That is to say your plating may be suspect.
Also, see if your etchback attack is more severe on prereg, so that the
plating looks like "ACCORDIAN". This, even if your plating quality is good
(tensile elongation strengths), may cause barrel cracks. This is very common
for plating cracks.
The root cause of differential etch-back lies somewhere else. Are prepreg
and core from same supplier ?. Is the prepreg completey cured ?
Good luck
Rush
Accurate Engg Inc.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|