TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 9 May 2008 17:40:54 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Neil Atkinson <[log in to unmask]>
Subject:
From:
Neil Atkinson <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (57 lines)
Thanks Werner,
 
If I solve this problem, I may have time to attend one of your seminars here
in the UK!
 
Neil

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: 09 May 2008 16:16
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] Fw: [TN] Brittle FPC Tracks


Hi Neil,
No such standard exists or can exist, because [drum roll]-'It depends!'
It depends on thicknees of the layers [each one individually], the modulus
of elasticity [of each layer-from this the location of the neutral plane is
determined], and the ductility of each metallic layer [use IPC-TM-650,
2.4.2.1 "Flexural Fatigue and Ductility, Foil," or ASTM  E 796 "Standard
Test Method for Ductility Testing of Metallic Foil"].
Having all of this, you can determine the minimum sustainable bend radius.
You can find the methodology in IPC-D-330, Section 6.2.1.2 "Flexibility
Considerations in the Design of Flexible Printed Wiring"  [most likely
out-of-print] or in the upcoming book by Joseph Fjelstad Flexible Circuit
Technology, 4th edition.

Werner
Future workshops:
Reliability Issues with Lead-Free Soldering Processes, June 17, London
Interconnect Failures and Design for Reliability for PCB PTHs, June 17,
London
Pb-Free Soldering Processes-Survival, Quality, Reliability, August 18,
Orlando
Reliability Issues with Lead-Free Soldering Processes, September 22,
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture,
ENIG), September 22, Schaumburg



**************
Wondering what's for Dinner Tonight? Get new twists on family favorites at
AOL Food.
(http://food.aol.com/dinner-tonight?NCID=aolfod00030000000001) 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2