TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Phillip E. Hinton" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 25 Nov 1998 18:15:27 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (23 lines)
Ken

I must assume that you are talking about Pb95/Sn5 and Pb10/Sn10.  Some
conventions always place the tin first and other place the major element
first.  Different countries use different conventions.  A good reference is J-
Std- 006 which for Pb95/Sn5 gives the solidus temperature at 208'C and the
liquidus temperature at 212'C, and for 90Pb/10Sn the liquidus temperature is
275'C and solidus temperature is 302'C.

Phil Hinton

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2