     Dwayne,                                                               
     Have you tried selective soldering fixtures where you drop a board in 
     vs putting sleeves on.                                                
                                                                           
     Been There                                                            


______________________________ Reply Separator _________________________________
Subject: Glass Epoxy Gold Finger Guards
Author:  "Dewayne Dunn" <[log in to unmask]> at uucpmail
Date:    12/27/96 14:22


>Message was resent -- Original recipients were: 
To:
[log in to unmask]
--------------
Dear IPC,
     
     We are looking for sources or vendors for glass epoxy gold
finger guards and connector covers to use in the wave solder process. 
We are already aware of Stevens Products but we are interested in other 
sources.  Please send any known  sources.
     
Thanks,
     Dwayne
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2