TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Kathy <[log in to unmask]>
Date:
Wed, 30 Nov 2005 07:37:58 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard" <[log in to unmask]>
Parts/Attachments:
text/plain (68 lines)
The surface finish becomes important as part of the dielectric at
frequencies above 1 gigahertz.
The Hall effect becomes more pronounced at high frequencies, and thus
the surface resistance is more of a factor in signal loss. Electroless
nickel has a much higher loss in Db/cm than HASL. The copper thickness
also plays an important role in overall conductivity above 1 ghz. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kathy
Sent: Tuesday, November 29, 2005 5:01 PM
To: [log in to unmask]
Subject: [TN]

I am posting this ? for a colleague:



"We are fabricating some boards for a customer that will be 1 oz of
copper on Duroid 6010.  They are considering two surface finishes:  HASL
(Hot Air Levelled Solder) and 150u" Nickel under 5-10 u" Gold.



The question they are asking is as follows:  What are the dielectric
properities of the Nickel/Gold finish vs. those of the HASL finish.



Does anyone know the answer?  I figured that the insulating material
(the
Duriod) and the conductor thickness (copper) would have the largest
influence on dielectric performance and that the surface finish would
have a negligible impact on performance.  Is this true?"



Thanks!








---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2