George,
I am not a fabrication expert, but I always thought that the palladium
was used only in the ENEPIG finish. Is it always used when plating ENIG
as well?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad
Sent: Wednesday, September 20, 2006 8:56 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG Skip Plating
Skip Plating is a term used to describe the absence of Ni deposition on
a pad surface.
It is occasionally encountered in processing parts down an ENIG line. It
is not the norm, and that is why ENIG continues to be a viable surface
finish with increasing market share.
Skipping in the Ni occurs when the palladium catalyzation on the copper
surface fails. Without the immersion Pd coating on the copper pads Ni
deposition does not initiate.
Pd is deposited on the Cu surface by an immersion exchange reaction. In
this reaction the cupper gives up an electron and is oxidized to the Cu
ion and goes into solution and the Pd ion in solution picks up the
electron and is reduced to the metal and deposited on the copper
surface.
The times that this reaction fails to proceed is when the copper surface
carries a delta charge that interferes with this electron transfer.
usually some form of a localized galvanic setup. This charge would be
shared by other pads on the same net.
Things that are known to cause this are:
Entrapped residual oxidant in a partially plugged via adjacent to the
pad that skips.
The presence of residual tin in the hole. Tin is used as an etch resist
and must be stripped.
The awareness of those 2 mechanisms, would go a long way in eliminating
the problem where it occurs.
I hope this helps.
Regards
George Milad
National Accounts Manager for Technology Uyemura International Corp
(UIC)
249 Town Line Rd
Southington CT 06489
[log in to unmask]
Cell: (516) 901 3874
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|