TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 19 Mar 2001 11:56:55 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (94 lines)
Hi, Earl,

The only problem I know of with electrolytic gold vs. solderability is that
it tends to make solder joints brittle if not first removed prior to the
soldering process - maybe that's the reason for the thin gold plating
specified now.

Regards

Pete Duncan
Asst Principal Engineer
ST Aerospace




Earl Moon <[log in to unmask]>@IPC.ORG> on 03/18/2001 07:45:36 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Earl Moon <[log in to unmask]>

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:
Subject:  [TN] CAM& AU




Folks,

I've never found an adequate/inexpensive CAM viewer/editor for .brd, from
Allegro, files. I know Valor does it and I know many others have asked the
same question but to no avail. Does anyone have a CAM package capable of
viewing and running DRC's on Cadence design stuff without having to pay
through the nose, or other orifices, and without having to rely on ODB ++
output as in CAM350's case.

Also, never done electrolytic gold over nickel for SMT. Assuming it is
similar, concerning solderability minus black stuff problems, to immersion
gold in that it gets the job done good or bad. Can't understand why my
current supplier goes outside for immersion and has the same thickness
electrolytic gold capabilities in house.

First, has anyone stories to tell about electrolytic gold and its
properties
pertaining to solderability? Do I have to worry about black pad? Why is 2
millionth's gold over about 200 millionth's nickel now the preferred
standard? Used to be 4 over 120, or so, was the nominal. Man/woman, that's
seems a lot of nickel with extremely littl gold over it.

Looked back at some postings, too many to count, and found Dave Hillman's
January posting to be most useful concerning thickness versus absorbtion
and rates, etc. Same holds true for electrolytic, I'm sure as we're talking
thickness, right? What about porosity versus thickness versus absorbtion
into the solder joint versus solder joint quality and reliability.

Makes me yearn for Entek again no matter the visual, cleaning, life,
storate, test, and all the other issues. Hell, It's flat and solders well
even if it gets the pogo pins abit gummed up.

Help appreciated - for us all insane folks in a diaganol world. Or, is
everyone else really in a parallel world as Jack Crawford told me. If
so, I'll park where I please. Damn, could be personal problem!

Earl Moon

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2