TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Fri, 11 May 2007 16:06:51 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (120 lines)
 
http://rf-shielding.com/specs.html


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Friday, May 11, 2007 3:32 PM
To: [log in to unmask]
Subject: Re: [TN] RF fences, oldering

Thanks Richard!

Can you elaborate a bit on the mechanical clip and the snap-and-twist? I
would certainly get rid of the soldered fences if the RF engineer would
agree and I would certainly like to show him the alternates.

Steve G already mentioned
http://www.autosplice.com/catalog/Page_21-22.PDF and I suppose this is
the mechanical clip.

Do you have anything else? Snap-and-twist?

Best regards,

Ioan

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stadem, Richard D.
Sent: Friday, May 11, 2007 4:18 PM
To: [log in to unmask]
Subject: Re: [TN] RF fences, oldering


You can probably use tin-plated steel for the fence, but you may not
want to. The tin can certainly be plated directly to the steel, but it
would have to be of such thickness that there would be no risk of
complete dissolution into the solder, else you have nothing to solder
to. I am not sure if this is practical or possible. I am assuming you
want a wet-joint connection (fully-soldered) along the ground plane on
the board, not a mechanical clip or snap-and-twist.
Secondly, Kester recommends against using tin-plated steel or brass for
shielding fences. Tin-plated steel is plated at the mill and then after
the fences are cut out you have a lot of exposed edges that corrode
quickly. You need slightly higher temperatures to solder to tin-plated
steel, and when you already have a high-mass steel fence the soldering
becomes so difficult that after repeated attempts there is no more tin,
and guess what happens then? 
I would use a .16 micron nickel barrier covered with Sn97.6Cu2.4 if I
had to use steel fences. I personally prefer nickel-plated brass. Have
the fences cut first and then nickel plated to cover all exposed basis
metal.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Friday, May 11, 2007 12:02 PM
To: [log in to unmask]
Subject: [TN] RF fences, oldering

Hi everybody,

since I had no answer to my question regarding the required thickness of
the Cu layer on top of a steel fence, I try to reformulate.

Can a fence be Sn plated steel only, with no Cu or Ni in between? Would
this solder, since Fe is practically insoluble in Sn, so there will be
no IMC?

Thanks,

Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2