Hi Steve
We manufacture both masking boots and don't use any oils in the process as
it does effect the dewetting on the pcb.
You can contact me off line for further information
Best Regards
Dr Lee Hitchens
SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21
www.conformalcoating.co.uk
TECHNICAL SUPPORT SERVICE
SCH Services Ltd offers a Technical Support Helpline to help address all
issues relating to reliability. This includes contamination testing,
cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
[log in to unmask] +44 (0)1226 249019 (office hours &
answerphone) +44 (0)7862 253321(out-of-hours emergency)
The opinions expressed in this e-mail are strictly those of the sender and
not of SCH Services Limited. This communication may contain information
which is confidential and may also be privileged. It is for the exclusive
use of the intended recipient(s). Unauthorised use, copying or disclosure
of any of it may be unlawful. If you are not the intended recipient(s)
please note that any distribution, copying or use of this communication or
the information in it is strictly prohibited. If you have received this
communication in error please notify us by e-mail or by telephone (+44
(0)1226 249019) and then delete the e-mail and any copies of it. Virus
Warning - Although steps have been taken to ensure that all email and
attachments are virus-free, we cannot guarantee nor be held liable.
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way
Barnsley South Yorkshire S70 6BF
On 14 Apr 2015 21:52, "Steve Gregory" <[log in to unmask]> wrote:
> Hi All,
>
> Just got some black ESD rubber masking boots for some blade terminals for a
> board that we dip in Humiseal 1A33, and noticed that there is shadowing
> around the base of the terminals like something was repelling the coating
> away from them, maybe some sort of mold release compound? Tried dipping
> without the boots and we don't see the shadow. I got the boots to keep the
> coating from getting on the terminals so that we weren't sitting there with
> a conformal coat removal pen cleaning the terminals up after we dipped the
> boards.
>
> I called the manufacturer of the boots and asked about the issue, and he
> said they would get back to me. Haven't heard anything yet. I'll try to get
> a picture that shows you what I'm talking about...
>
> Steve
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|