TECHNET Archives

April 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brian Ellis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Wed, 1 Apr 2015 16:38:09 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (12 lines)
The Institute of Waste Reduction in Electronics in Germany have made a 
proposal to the EU that the next review of RoHS incorates a clause to 
ban all through-hole components. This is because the amount of solder 
and flux used is twice as much, compared with surface-mount components. 
They also propose re-introducing lead into solder pastes as they 
consider the easier wetting of 63/37 produces smaller fillets.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2