TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 6 Aug 2008 11:35:31 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
MIME-Version:
1.0
content-transfer-encoding:
base64
Content-Type:
text/plain; charset="UTF-8"
From:
Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
As far as I can recall there is a difference of slightly longere time above liqudus, and surface tension , which produce better soldering results.  However, without knowing the specific application requirement, any selection is shot in the dark.  

--------------------------

Sent using BlackBerry





----- Original Message -----

From: TechNet <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Wed Aug 06 10:25:53 2008

Subject: Re: [TN] SOLDER FOR PCB  REFLOW PRO CESS



Hi Ben,

Actually, it has never been proven that Sn62/Pb36/Ag2 prevents leaching on 

components finished with silver—it appears to sound reasonable, but is an urban 

myth.

Sn62/Pb36/Ag2 is somewhat stronger [which is totally without practical value—

and the still stronger SAC-solders cause pad cratering] than Sn63Pb and has a 

slightly lower Solidus/Liquidus temperature. Creep-fatigue-wise there is no 

significant difference.



Werner

Future workshops:

Reliability Issues with Lead-Free Soldering Processes, September 22, 

Schaumburg

Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture, 

ENIG), September 22, Schaumburg

Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia

Solder Joint Reliability: Part 4, Oct. 17, Timisoara, Rumania

Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia







**************

Looking for a car that's sporty, fun and fits in your budget? 

Read reviews on AOL Autos.

      

(http://autos.aol.com/cars-BMW-128-2008/expert-review?ncid=aolaut00050000000017 )



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.


ATOM RSS1 RSS2