TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wee Mei <[log in to unmask]>
Date:
Fri, 13 Oct 2006 08:37:57 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (127 lines)
        Wee Mei:
                   On the bolt head side, use a flat washer. On the nut
side,  use  flat washer, lock washer and lastly the nut. The lock washer
regardless of the type, star, split.. should not deform the PWB.
        Regards,
        Ramon
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wee Mei
Sent: Thursday, October 12, 2006 6:46 PM
To: [log in to unmask]
Subject: Re: [TN] Compression Limit on FR4?

Hello,

I happen to be trouble with screws and nuts on the PCBA recently. Can
someone point to a site to show how mechanical hardware assembly
installation is carried out on PCBA?

I have come across all sort of assembly configuration on just the screw,
washers and nut on PCBA that I did not know which is correct. Different
engineers used different method and even different screw or nuts on the
same build PCBA. What should be correct hardware assembly configuration.

Thanks and regards,
Wee Mei


----- Original Message -----
From: "Stadem, Richard D." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, October 13, 2006 3:02 AM
Subject: Re: [TN] Compression Limit on FR4?


> Hi, Jack
> I can tell you that typically the torque setting used for hardware on
> pwb assemblies is between 1 to 6 in/lbs. More than that tends to
deform
> the fiberglass over time. Of course, it all depends on the type of
board
> material, layer count, etc.
> It also depends on the application.
> Realize that a lot of relaxation occurs during any type of thermal
> excursion, and the hardware will loosen up. It is always a good idea
to
> use a Bellville washer in conjunction with a serrated or star washer
to
> continue to hold the torque. It is also a good idea to use Glyptol or
> some other threadlocker. 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
> Sent: Thursday, October 12, 2006 1:54 PM
> To: [log in to unmask]
> Subject: [TN] Compression Limit on FR4?
> 
> Does anyone know of any guidelines or recommendations that suggest a
> maximum limit on compressing board material?
> 
> Can any damage occur by over-torque'n screws, for example?
> 
> I've never heard anyone discuss that...
> 
> Jack
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2