TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
Date:
Wed, 14 Sep 2005 12:39:40 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (144 lines)
method (drinking dew) not comply with mil-std-xyz... in valid... almost
chock myself (no air in-let step etc.etc. ;-)... by the way, even it is
insufficient method, since it is out open in TechNet, it is common knowledge
and no longer patentable by Doug P...hehehe.
                          jk

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Douglas O. Pauls
Sent: Wednesday, September 14, 2005 11:42 AM
To: [log in to unmask]
Subject: Re: [TN] Comb Pattern PCB


Joyce,
For a commodity item, like a B-24 board, which is used for materials
studies, they can come from almost any source.  Yes, it is best that you
get them from one of your regular suppliers and IPC (or I) can provide the
Gerber files, if for no other reason than you can sometimes  see if you
have a crappy fab house before investing money in actual product.  It
becomes more important that you have the test boards made by your vendor
when you are doing process qualification or characterization work.  In that
instance, you want the same laminate/mask/metalization/marking ink scheme
intended for actual product.  And if you get crappy results, and you show
that your supplier is crappy, you can avoid some pain on actual product.
At least in theory.

As for the Dew.  grasp bottle firmly in left hand, twist off cap, give cap
to young co-worker foolish enough to believe that he has a shot in winning
the X-box prize, raise bottle to lips, upend, swallowing in a rate to
approximately equal the incoming flow rate.  Repeat as necessary.
Hallucinations optional.

Doug Pauls




             Joyce Koo
             <[log in to unmask]
             COM>                                                       To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             09/14/2005 07:53          Re: [TN] Comb Pattern PCB
             AM


             Please respond to
             [log in to unmask]
                    om






I thought you have to get your vendor to do the comb....not from someone
else...
If you get comb from vendor A PCB and pass the SIR, is it equal to vendor B
PCB can pass the SIR?  Doug, could you teach me drink some dew?
                             jk

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jim Smith
Sent: Wednesday, September 14, 2005 1:34 AM
To: [log in to unmask]
Subject: [TN] Comb Pattern PCB


Hello, all.

Does anyone know of a supplier with stock comb filter pattern PCB's for
SIR testing?

Thanks in advance for the help.

Best wishes,

Jim
--------------------------------------------------------------------------
Jim Smith
Managing Director
Electronics Manufacturing Sciences, Inc.
4285 45th St. S.
St. Petersburg, FL 33711-4431
Tel: (727)866-6502,  Ext. 21
Mobile: (727)542-0789
Fax:  (727)867-7890
E-mail:  [log in to unmask]
www.emsciences.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------