TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Barton <[log in to unmask]>
Date:
Wed, 26 Sep 2012 10:35:37 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (69 lines)
Hi Peter - I agree with Vlad, we still have a mixed metallurgy situation 
for the solder joint so I would treat it as having the same solder joint 
integrity concerns that would need to be reviewed and assessed.

Dave



Peter Barton <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
09/26/2012 09:45 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Peter Barton    <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Using Tin/Lead balled BGA in a Lead-Free process






Hi Technetters,

Interesting that this question has arisen for me when there has been a 
question posed here on the reverse scenario in the last couple of days. 
Firstly, I agree with other posters that full reflow and alloy mixing must 
be achieved when using Lead free BGA's in a Tin Lead process. There is 
quite a lot of data out there supporting this.

My problem is finding research data on using a Tin/Lead BGA on an 
otherwise fully Lead free assembly. This appears to be much more limited. 
So far I have only found one paper that refers to this particular scenario 
and some of it's conclusions are carefully qualified. 

Assuming that all the other the packaging materials for the Tin/Lead BGA 
part in question are capable of surviving a suitable reflow process to 
successfully solder the lead free parts whilst minimising thermal input, 
can anyone out there comment on potential reliability issues. For 
information the BGA balls are 63/37 Sn/Pb and the solder paste alloy is 
SAC305.

Many thanks in advance,

Peter Barton






______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2