Hi All:
I am working in a PCB fabricator in China, and we scarcely heard the
similar case form our SMT customers, we have all kinds of surface finish
process, such as OSP, HASL, Immersion gold and so on..... I think this is
properly the problem from the solder mask; we use DI water clean the boards
after solder mask and have UV "bump" during mask cure, I think this will
helpful.
Winning
-----邮件原件-----
发件人: TechNet [mailto:[log in to unmask]] 代表 Wenger, George M.
发送时间: 2009年5月7日 21:34
收件人: [log in to unmask]
主题: Re: [TN] PB Surface Contamination
What is the surface finish on the PCB? If it is HA
Joe,
What is the surface finish on the PCB? If it is HASL there is a reason
for the contamination.
Regards,
George
George M. Wenger
Andrew Wireless Solutions
Senior Principal FMA/Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 (Office) (732) 309-8964 (cell)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
SSA)
Sent: Thursday, May 07, 2009 9:13 AM
To: [log in to unmask]
Subject: [TN] PB Surface Contamination
A cleaned bare PB is exposed to bake or reflow, and comes out with
measurable ionic contamination. The board is dirtier at the surface
after
a heat excursion.
The contamination isn't coming from the oven, handling, or anything
external.
Heat causes something to move from the inside of the board to the
outside.
We haven't done any ion chromatography or other testing yet to
run this down, but has anyone heard of or experienced anything similar?
In our normal process, we clean everything multiple times, but if the
contaminant builds up under solder mask, or in other areas that are
difficult to clean, we could have SIR or corrosion problems around fine
surface features or in high voltage areas.
And if this ionic contamination doesn't just move up to the surface,
but is somehow moving around inside the board, could it collect in
some places and lead to CAF or other problems?
Joe Kane
BAE Systems
Johnson City, NY
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
----------------------------------------------------------------------------
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
----------------------------------------------------------------------------
--------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|