     Hi Kirk -
     
     Take a look at the following reference: "Parametric Study on the 
     Solderability of Etched PWB Copper", F. Hosking, SMI Proceedings 1996, 
     page 671. The paper (and its references) contains quite a bit of info 
     on surface tension and wetting of thin lines that may be of use to 
     you. Good Luck.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]
     
     


______________________________ Reply Separator _________________________________
Subject: 90/10 to 63/37 SnPb Comparison
Author:  [log in to unmask] at ccmgw1
Date:    5/21/97 12:08 PM


     
     
     
Kirk VanDreel
05/21/97 12:02 PM
Does anyone know of papers, books or proceedings which compare the surface 
energy and flow characteristics between 90/10, 85/15, and 63/37 plated 
SnPb?
     
Thanks,
Kirk Van Dreel
Hutchinson Technology
[log in to unmask]
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2