Nee hao Min Jun,
Now that you say "nickel" and "brittle failure"in one breath, the likelihood
that you have ENIG's 'back pad' is retty strong. In these cases, the
interface between the Ni and the IMClayers is weakened, and sfficient loading causes
brittle failure.
You should be attending my workshop dealing with this issue this coming
Monday at IPC Midwest Conference.
Regards,
Werner Engelmaier
可靠性先生
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************
Looking
for simple solutions to your real-life financial challenges? Check out
WalletPop for the latest news and information, tips and calculators.
(http://www.walletpop.com/?NCID=emlcntuswall00000001)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|