TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 17 Apr 2008 16:51:01 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier /* <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
Hi Terry,
The materials under these slash sheets may or may not be 'RoHS-compliant', 
but with the exception of /99 they are not 'RoHS-capable'. That means that their 
STII (Soldering Temperature Impact Index)-values are too low. /99 gives a 
minimum STII of 202, which would make that material of limited usefullness for 
lead-free soldering processes—there are however materials under slash /99 that 
have higher STII values.
For more information—a lot more information—you should be getting my White 
Paper: "Recommendations for PCB FAB Notes and Specifications in Printed Circuit 
Board Drawings for SnPb and Lead-Free Soldering Assemblies, the Qualification 
of PCB Shops and Activities to Assure Continued Quality."

Werner



**************
Need a new ride? Check out the largest site for U.S. used car 
listings at AOL Autos.
      
(http://autos.aol.com/used?NCID=aolcmp00300000002851)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2