So far as I recall the original "red Jelly" flux was made by Fry way back when and was, possibly
still is, basically a heat stabilised RMA+/RA- resin. Although originally a non electronic
material it was then pretty good especially for things like high lead alloys, but I would think
that modern tack (paste) fluxes are equivalent. Multicore may have resurrected this product or
it could be an entirely novel development. Perhaps they will
let us know?
Mike
----- Original Message -----
From: Pat Diamond <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 09, 2000 3:08 PM
Subject: [TN] "Red Jelly" Flux
> Hi,
>
> Can anyone supply information on Red Jelly flux?, I know that it is made by
> Multicore and is Rosin based.
> Does anybody out there have any experience of using this as it looks like it
> could be ideal for one of our processes. I would also like to know how
> active/agressive this jelly is and what cleaning medium is required as my
> contact at Multicore just keeps telling me it's the best thing since sliced
> bread!.
>
> Thanks in advance
>
> Pat Diamond
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|