TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wozJm-000BjaC; Thu, 17 Jul 97 17:46 CDT
Old-Return-Path:
Date:
Thu, 17 Jul 1997 18:57:20 -0400 (EDT)
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
>From willli Thu Jul 17 17:
46:55 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"am2Ix2.0.KyK.D3gpp"@ipc>
From [log in to unmask] Mon Jul 21 15:
57:49 1997
From:
X-Mailing-List:
<[log in to unmask]> archive/latest/14100
X-Loop:
Subject:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (25 lines)
jim -

there is a difference between low copper adhesion - UNDERPLATE - and poor
copper adhesion. Check exposing to meet parameters - check strength of
developing solution - Check pressure spray on developer - Check actual
nozzles - Check breakpoint on developer - Check cleaner - Check condition of
copper bath - without definite info as to what is occurring - hard to come up
with a pinpointed answer. Hope this helps.

Regards

Richard Fudalewski
Atotech Canada Ltd

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2