Hello in there,
No, you do not need to worry about losing bits off the bottom during second
reflow. The surface tension of liquid solder is more than enough to keep
little passives in place. All my boards have many, many passives underneath
and a few IC's besides, and they all hang on there perfectly.
Peter
STAero
ART HAMPTON
<smt@Q-TRONIC To: [log in to unmask]
S.NET> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: Aero/ST Group)
TechNet Subject: [TN] Bottom Side Reflow!!
<[log in to unmask]
ORG>
03/07/02
05:00 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
ART HAMPTON
Hello Out There,
Recently I was assigned the task of creating profiles that would fall
within the ( PWI ) for solder paste Kester ( 562 ) for processing pcbs
with several (bga) components on the top side, however the bottom side
of the pcb also has 1,200 placements of cap, and res. reflowed not
epoxyed, do I need to be worried about losing my bottom side components?
Art
____________________________________________________
(Embedded image moved to file: pic13944.gif) IncrediMail - Email has
finally evolved - Click Here
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|