TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Landman <[log in to unmask]>
Date:
Tue, 22 Oct 2013 17:58:38 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Message-ID:
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (51 lines)
You need an etchant containing a strong sodium hydroxide, ammonia and 
tetrahydrofuran, which will remove the outer fluorine atoms, leaving an 
electrically charged surface that will bond to adhesives. However, this 
is a very toxic, caustic, really nasty stuff and your H&S guys will 
baulk at its use, after the first operator drops dead! In addition, I 
think that removing the residues after etching and before glueing will 
be electrically ultra-problematic.

I would suggest that mechanically abrading would really be your best 
compromise, hopefully providing a key to a low-viscosity solvent-free epoxy.

Brian

On 22.10.2013 17:21, Bob Landman wrote:
> Bob,
>
> McMaster Carr supplies a Teflon epoxy system which has a liquid etchant to prepare the surface for their two component epoxy. Its packaged in a circular cardboard box with a screw top lid.  We've used it to bond Teflon to aluminum for decades. Don't know if it works on epoxy/resin boards but as it can bind Teflon to Teflon (another app we have a requirement for) give them a call to see what they recommend.
>
> Bob Landman
> H&L Instruments,LLC
>
>
> Sent from my iPhone
>
> On Oct 22, 2013, at 10:09 AM, Bob Wettermann <[log in to unmask]> wrote:
>
>> Can a chemist/board SME tell me if an epoxy/resin system will bond to a PTFE
>> matrix laminate for pad/trace repair?
>>
>> Thanks!
>>
>> Bob Wettermann
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2