Keith,

Regarding your October message about soldering gold pcb's in a
nitrogen convection reflow oven:

Have you checked the O2 level in the oven lately?  It's quite common to have
O2 levels of several percent due to room drafts etc.

Mark Nowotarski
Manager - Soldering Atmospheres Development
Praxair Inc.
Tarrytown NY USA