Hi Charming,
What you have is a PCB made of CEM-1 or -2 with unsupported holes---this is Class -1(minus 1) not Class 2.
While this might work for some applications, you cannot claim that you have a Class 2 product; and in harsh environments you clearly will have problems.
Werner
-----Original Message-----
From: Charming Chan <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, Nov 19, 2009 3:37 pm
Subject: [TN] Discussion on the reliability of single-sided PCB & PCBA
Hello All,
Our power system suppliers build single-sided pcb with paper-based substrates,
he holes on the pcb are non-plated and no solder fill for through-hole
omponent. As I know, paper-based substrates are generally used for the pcb
uild of low-cost, low-reliability, consumer products.
Our company sells CLASS 2 networking products, which are supposed to work in
arsh environment. Is it reliable enough to use such single-sided power
ssembly? Thanks a lot for kindly input.
Best Regards
harming Chan
--------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
dditional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|