Steve,
I understand what you are saying, but Peter spoke specifically about a
possible alloy effect and I was trying to get some more info about that.
Bev
-----Original Message-----
From: Creswick, Steven [mailto:[log in to unmask]]
Sent: April 10, 2002 12:21 PM
To: [log in to unmask]
Subject: Re: [TN] 0402 tombstone problem
Could it be that rather than Sn/Pb composition, it might be related to the
wettability (prior storage conditions) of the components in question -
thereby tying it into the required activity level of the flux?
Considered rectangular pads with rounded corners, or 'rectangular' pads with
semi-circular ends? It has worked on LTCC based product.
Steven Creswick - Gentex.Corp
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Wednesday, April 10, 2002 8:46 AM
To: [log in to unmask]
Subject: Re: [TN] 0402 tombstone problem
Peter,
So which is worse - high tin (e.g. Sn/Pb95/5) or relatively "high" lead
(Sn/Pb63/37)?
Bev Christian
Research in Motion
-----Original Message-----
From: Peter Lee [mailto:[log in to unmask]]
Sent: April 10, 2002 12:07 AM
To: [log in to unmask]
Subject: Re: [TN] 0402 tombstone problem
Our experience with eliminating 0402 tombstoning was to try different
no-clean solder paste. We've also found that the parts' end termination
tin/lead % has some negative impact on the yield.
Rgds,
Peter
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: April 9, 2002 8:13 PM
To: [log in to unmask]
Subject: Re: [TN] 0402 tombstone problem
I just heard something not too long ago, that round pads for 0402's are the
way to go.
Never heard of that before, but just recently received a board for quote
that uses round pads for the 0402 components...anybody else ever heard of
this?
Guess I'll find out how it works inna little while, while pondering why a
round pad would work better than a square pad....
-Steve Gregory-
Edward,
When we do everything correct on 0402 and 0201 and still have components
standing-up, we often look to the component terminations and find poor
plating.
Good luck
Dave Fish
----- Original Message -----
From: "Edward S. Wheeler" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, April 09, 2002 10:59 AM
Subject: [TN] 0402 tombstone problem
> Hi folks, we are running a new board with 0402 parts on it. It seems that
> we are having a tombstone problem as well as a problem with parts not
> staying centered on the pads. We are currently using 20 mil square pads on
> the board, with 20 mils of spacing between them. Our stencil is 6 mils
> thick, laser cut and electro polished. The trapezoidal walled apertures
are
> slightly reduced, 17 mils square, and centered on the pads. It appears the
> chip shooter is placing the parts perfectly. We are using eutectic solder
> paste with an OA flux, and reflowing the parts using the recommended
profile.
>
> Are there any suggestions any of you might have concerning this size of a
> part? Is there a better stencil design, reflow profile, or pad design that
> could help us out? I would appreciate any suggestions.
>
> Thanks.
>
> Ed
|