You mean IPC-6012, right? Table 3-2 it sounds like. I don't see that
requirement listed in the IPC-A-600.
We're a fab, not an assembler, but I've heard of significant reliability
problems with holes having less than .0007 (18 micron) copper in them. I
would stick to the spec. (My $.02)
Tim Reeves
|-----Original Message-----
|From: Ashley Allen Shepard [mailto:[log in to unmask]]
|Sent: Friday, March 09, 2001 6:49 AM
|Subject: Exception to IPC-A-600 Class II minimum via wall plating
|
|
|Hi All,
|
|I'm wondering if anyone has data they'd be willing to share
|supporting the
|18 micron minimum (class I and II) Final Finish, Surface
|Plating Coating
|Requirements in the IPC-A-600 specification. Specifically,
|I'm interested
|in the effects of reducing via wall plating thickness. Any information
|would be greatly appreciated.
|
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|