TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 13 Jul 2009 10:00:23 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Subject:
From:
Dwight Mattix <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (254 lines)
At 09:27 AM 7/13/2009, Joyce Koo wrote:
>Not totally true.  You have lived long enough to know better?

yep and to know that .gov involvement usually makes for a similar 
scale but much more deeply calcified problem. I know which bias I prefer.

Now in Texas they've got the streamlined solution.  It's a positive 
defense for misdemeanor battery.

"I reckon he (the HR rep?)  just need a beatin' yer Honor."

>--------------------------
>Sent using BlackBerry
>
>
>----- Original Message -----
>From: TechNet <[log in to unmask]>
>To: [log in to unmask] <[log in to unmask]>
>Sent: Mon Jul 13 12:09:50 2009
>Subject: Re: [TN] NTC: I just joined the ranks of the unemployed...
>
>At 08:19 AM 7/13/2009, Lee parker wrote:
> >Dean
> >
> >Your comments are interesting, but in many states this is certainly
> >not the case. Employers can be as abusive as they desire.
> >
> >What is the particular stature which prohibits this behavior;
>
>The market.
>
> >  I certainly believe such a probation is needed.
> >
> >Lee
> >   ----- Original Message -----
> >   From: Stadem, Richard D.<mailto:[log in to unmask]>
> >   To: [log in to unmask]<mailto:[log in to unmask]>
> >   Sent: Monday, July 13, 2009 11:06 AM
> >   Subject: Re: [TN] NTC: I just joined the ranks of the unemployed...
> >
> >
> >   Three years ago.
> >
> >   -----Original Message-----
> >   From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
> >   Sent: Friday, July 10, 2009 11:30 AM
> >   To: [log in to unmask]<mailto:[log in to unmask]>
> >   Subject: Re: [TN] NTC: I just joined the ranks of the unemployed...
> >
> >   What century do you talk about?
> >   /Inge
> >   ----- Original Message -----
> >   From: "Dean Stadem"
> > <[log in to unmask]<mailto:[log in to unmask]>>
> >   To: <[log in to unmask]<mailto:[log in to unmask]>>
> >   Sent: Friday, July 10, 2009 6:05 PM
> >   Subject: Re: [TN] NTC: I just joined the ranks of the unemployed...
> >
> >
> >   > Hi, Ken
> >   > That is now illegal. There are specific methods of informing survivor
> >   > employees AFTER the layoff has occurred. The law is very clear on
> >   this.
> >   >
> >   > I once had a manager who came to work dressed in a long black gown,
> >   > wearing a black hood and mask, and carrying a scythe. He would walk up
> >   > behind the employee to be laid off, tap him/her on the shoulder, and
> >   > crook his finger and say, "Your time is up, my friend. Gather together
> >   > your personal belongings and come with me".
> >   > The day after he was finished laying people off, they fired his ass
> >   and
> >   > he was escorted out of the building.
> >   > They ended up paying umpteen million bucks in the class-action lawsuit
> >   > brought about against them for this manager's antics.
> >   >
> >   > R. Dean Stadem
> >   > Consulting Engineer
> >   > Analog Technologies Corp./Lumagine, Inc.
> >   > 11441 Rupp Drive
> >   > Burnsville, MN 55431
> >   > (952)894-9228
> >   > [log in to unmask]<mailto:[log in to unmask]>
> >   >
> >   >
> >   > -----Original Message-----
> >   > From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
> >   > Sent: Friday, July 10, 2009 10:14 AM
> >   > To: [log in to unmask]<mailto:[log in to unmask]>
> >   > Subject: Re: [TN] NTC: I just joined the ranks of the unemployed...
> >   >
> >   > One of the worst layoff's I ever went through, even though I didn't
> >   get
> >   > laid
> >   > off, was a big one where HR would get on the PA every half hour or so
> >   > and
> >   > read off a list of the next terminations. This went on all day, very
> >   > nerve
> >   > wracking and a VERY long day!
> >   >
> >   > KennyB
> >   >
> >   > ---------------------------------------------------
> >   > Technet Mail List provided as a service by IPC using LISTSERV 15.0
> >   > To unsubscribe, send a message to
> > [log in to unmask]<mailto:[log in to unmask]> with following text
> >   > in
> >   > the BODY (NOT the subject field): SIGNOFF Technet
> >   > To temporarily halt or (re-start) delivery of Technet send e-mail to
> >   > [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
> >   > To receive ONE mailing per day of all the posts: send e-mail to
> >   > [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
> >   > Search the archives of previous posts at:
> >   > http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
> >   > Please visit IPC web site
> >   >
> > 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> 
>
> > for additional
> >   > information, or contact Keach Sasamori at
> > [log in to unmask]<mailto:[log in to unmask]> or
> >   847-615-7100
> >   > ext.2815
> >   > -----------------------------------------------------
> >   >
> >   > ---------------------------------------------------
> >   > Technet Mail List provided as a service by IPC using LISTSERV 15.0
> >   > To unsubscribe, send a message to
> > [log in to unmask]<mailto:[log in to unmask]> with following text
> >   in
> >   > the BODY (NOT the subject field): SIGNOFF Technet
> >   > To temporarily halt or (re-start) delivery of Technet send e-mail to
> >   > [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
> >   > To receive ONE mailing per day of all the posts: send e-mail to
> >   > [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
> >   > Search the archives of previous posts at:
> >   http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
> >   > Please visit IPC web site
> >
> >http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org 
> /contentpage.asp?Pageid=4.3.16>
> >
> >   > for additional information, or contact Keach Sasamori at
> >   [log in to unmask]<mailto:[log in to unmask]> or
> >   > 847-615-7100 ext.2815
> >   > -----------------------------------------------------
> >
> >   ---------------------------------------------------
> >   Technet Mail List provided as a service by IPC using LISTSERV 15.0
> >   To unsubscribe, send a message to
> > [log in to unmask]<mailto:[log in to unmask]> with following text
> >   in
> >   the BODY (NOT the subject field): SIGNOFF Technet
> >   To temporarily halt or (re-start) delivery of Technet send e-mail to
> >   [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
> >   To receive ONE mailing per day of all the posts: send e-mail to
> >   [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
> >   Search the archives of previous posts at:
> >   http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
> >   Please visit IPC web site
> >
> >http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org 
> /contentpage.asp?Pageid=4.3.16>
> >for additional
> >   information, or contact Keach Sasamori at
> > [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
> >   ext.2815
> >   -----------------------------------------------------
> >
> >   ---------------------------------------------------
> >   Technet Mail List provided as a service by IPC using LISTSERV 15.0
> >   To unsubscribe, send a message to
> > [log in to unmask]<mailto:[log in to unmask]> with following text in
> >   the BODY (NOT the subject field): SIGNOFF Technet
> >   To temporarily halt or (re-start) delivery of Technet send e-mail
> > to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
> >   To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
> >   Search the archives of previous posts at:
> > http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
> >   Please visit IPC web site
> > 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> 
>
> > for additional information, or contact Keach Sasamori at
> > [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
> >   -----------------------------------------------------
> >
> >---------------------------------------------------
> >Technet Mail List provided as a service by IPC using LISTSERV 15.0
> >To unsubscribe, send a message to [log in to unmask] with following text in
> >the BODY (NOT the subject field): SIGNOFF Technet
> >To temporarily halt or (re-start) delivery of Technet send e-mail to
> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
> >To receive ONE mailing per day of all the posts: send e-mail to
> >[log in to unmask]: SET Technet Digest
> >Search the archives of previous posts at: http://listserv.ipc.org/archives
> >Please visit IPC web site
> >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> >information, or contact Keach Sasamori at [log in to unmask] or
> >847-615-7100 ext.2815
> >-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to 
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site 
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>information, or contact Keach Sasamori at [log in to unmask] or 
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain 
>confidential information, privileged material (including material 
>protected by the solicitor-client or other applicable privileges), 
>or constitute non-public information. Any use of this information by 
>anyone other than the intended recipient is prohibited. If you have 
>received this transmission in error, please immediately reply to the 
>sender and delete this information from your system. Use, 
>dissemination, distribution, or reproduction of this transmission by 
>unintended recipients is not authorized and may be unlawful.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to 
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site 
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>information, or contact Keach Sasamori at [log in to unmask] or 
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2