TECHNET Archives

October 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Thierolf, Chris @ MPSG - SPD" <[log in to unmask]>
Date:
Fri, 30 Oct 2015 08:36:44 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Message-ID:
<044601d1130f$a2df85d0$e89e9170$@com>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
Cleanliness levels for rework are the same as for production. 
Attempting to remove no-clean flux residue can be very risky, much worse
than leaving it alone. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thierolf, Chris @ MPSG -
SPD
Sent: Thursday, October 29, 2015 7:44 PM
To: [log in to unmask]
Subject: [TN] Pierced Terminal

I'm seeking some input to a solder condition that gets scrutinized in many
directions. For the soldering of a stranded 10-12awg stranded wire to a
pierced resistor terminal, a no clean L0 or L1 (RO/RE) flux is used with
63/37 solder. This is a single solder joint on a panel mount resistor, so no
PCB involved. Flux residue is observed and assembly rejected by QC but
manufacturer claims its no worry, and no clean flux. My observation says it
presents no electrical or operational issue, not a violation of J-STD-001,
but perhaps a visual issue per IPC-A-610, sec 10.6.4 "Flux residue inhibits
visual inspection" if floor inspector claims he cannot see the solder joint
clearly, which has occurred. We can state "clean the solder joint"
(relatively speaking), but what really is clean in this case? Should we be
forced to inspect these joints with 4x mag, as some are doing, or generate a
simple guideline that allows residue up to a certain level? What is this
level?

I have a picture of a failed solder joint if interested, but not sure where
to upload.


______________________________________
[Disc3.png]
Chris Thierolf
Principal EE and Project Engineer
L-3 Electronic Systems Segment
SPD Electrical Systems
13500 Roosevelt Boulevard
Philadelphia, PA 19116
Phone: (215) 698-6390    Fax: (215) 677-4736


________________________________
CONFIDENTIALITY NOTE: This electronic transmission, including all
attachments, is directed in confidence solely to the person(s) to whom it is
addressed, or an authorized recipient, and may not otherwise be distributed,
copied or disclosed. The contents of the transmission may also be subject to
intellectual property rights and all such rights are expressly claimed and
are not waived. Unless specifically modified by L-3 SPD Electrical Systems ,
the content of this electronic transmission is to be read subject to L-3 SPD
Electrical Systems  standard terms of business. This electronic transmission
may be intercepted or affected by viruses and L-3 SPD Electrical Systems
accepts no responsibility for any interception or liability for any form of
viruses introduced by this electronic transmission. If you have received
this transmission in error, please notify the sender immediately by return
electronic transmission and then immediately delete this transmission,
including all attachments, without copying, distributing or disclosing same.

ITAR CONTROL STATEMENT: In the event this document (or any of the
enclosures) contains technical data within the definition of the
International Traffic in Arms Regulations or Export Administration
Regulations, it is subject to the export control laws of the U.S.
Government. Transfer of this data by any means to a foreign person, whether
in the United States or abroad, without an export license or other approval
from the U.S. Department of State or Commerce, is prohibited.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2