From:
sam mccorkel <[log in to unmask]>
Date:
Tue, 6 Jan 1998 12:25:53 -0500
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, sam mccorkel <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
We're experiencing a problem that could be described as similar to "dishdowns".

For now we're calling them "squigglies".

        The circuit has an indentation in the copper that appears to be an
area that did not plate copper while pattern plating. The areas are small
and have a somewhat circular shape with only the perimeter being devoid of
plated copper. The inside of this circular area did plate while pattern
plating. The base copper is still there.
        The circular shape and pattern could be something that leaked out of
the holes while they were racked at a previous process?

I'm hoping someone recognizes this condition and can help us out.

Thank you!

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2