TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Bergman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, David Bergman <[log in to unmask]>
Date:
Mon, 1 Jul 2013 12:48:52 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (51 lines)
Hi Selim,

After vacuum baking did you add desiccant and seal the board?  If the board is left open to ambient conditions, it will most likely absorb back everything that you baked/vacuumed out. 

Best regards, 
Dave

David W. Bergman
Vice President, International Relations
IPC - Association Connecting Electronics Industries
3000 Lakeside Drive Suite 309S Bannockburn, IL 60015-1249 USA
+1 847-597-2840 tel
+1 847-615-5640 fax
+1 847-867-1388 mobile
[log in to unmask]
Skype: davidbergmanipc
www.ipc.org


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Avni Selim Özçukurlu
Sent: Monday, July 01, 2013 6:36 AM
To: Technet
Subject: [TN] Moisture in PCB

Hello All,


 


After a wave solder process of a PCB with lots of through-hole components on it, I have seen that there are popcorn part near via on that PCB. The flatness of the first layer of the PCB is gone after that process. I think that moisture remaind inside PCB gets outsite during the wave solder process and cause this problem. I didn't put the PCB in a vacuum oven before wave solder. Is it possible that the problem is related of this. Is there any alternative solution about that problem?


 

Actually I applied the heat up and vacuum to empty PCB before all process of manufacturing. After that vacuum oven process, it has passed about 10 days to start the wave solder process. During that 10 days, did PCB get moisture inside?

 

Thank you advance.

 

Selim.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

ATOM RSS1 RSS2