TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Brad L. Matthies" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 10 Oct 2000 13:21:14 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (103 lines)
Side question,

Does anyone know of a formula which determines if the ball collapse will produce an
acceptable joint?  It probably takes into account the size to the array balls
(surface area, material makeup or whatever) along with the weight of the component.
Someone must have already looked at this to design the package initially, right?

blm

>         -----Original Message-----
>         From:   d. terstegge [SMTP:[log in to unmask]]
>         Sent:   Tuesday, October 10, 2000 9:59 AM
>         To:     [log in to unmask]
>         Subject:        [TN] Heavy BGA's, now it's fine-pitch !
>
>         Hi Technet,
>
>         I need your advice on this one:
>         Some time ago there was a discussion about soldering problems with
> partnumberTMS320C6201GJC200 of Texas Instruments. It's a 1.27 mm pich BGA
> with a heavy heat-slug on top. The weight of the heat-slug makes the
> solderballs collapse a little too much, resulting in solder bridges.
>         Now I've got to assemble some boards with similar parts, but with a
> much smaller ballpitch of only 0.8 mm.
>         No problem for the ordinary type BGA's, but with the heatsink I'm
> starting to feel uncomfortable. For the record: it's TI's part
> numberTMX320C6203GLS.
>         I've got to build two boards, and all I've got is two components. No
> trial and error possible......
>         If anyone of you have experience or thoughts about this, please let
> me know.
>
>         Kind regards,
>
>         Daan Terstegge
>         SMT Centre
>         Signaal Communications
>         Unclassified mail
>         Personal Website: http://www.smtinfo.net
>
> ----------------------------------------------------------------------------
> -----
>         TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
>         To unsubscribe, send a message to [log in to unmask] with following
> text in
>         the BODY (NOT the subject field): SIGNOFF TECHNET
>         Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
>         information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
> ----------------------------------------------------------------------------
> -----
>
> ----------------------------------------------------------------------------
> -----
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF TECHNET
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ----------------------------------------------------------------------------
> -----
>
> ----------------------------------------------------------------------------
> -----
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF TECHNET
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ----------------------------------------------------------------------------
> -----
>
> ---------------------------------------------------------------------------------
>
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF TECHNET
> Please visit IPC web site ((http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ---------------------------------------------------------------------------------
>
> ---------------------------------------------------------------------------------
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF TECHNET
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET