How to analyze the gold and cyanide concentration in potassium gold cyanide KAu(CN)2 ?
We use sulfuric acid to analyze gold now.
But when we heat the soltion , there are a lot of fume.
Are there any other mehtod to avoid producing fume?
Please give me the physical and chemical properties about potassium gold cyanide.