TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Macko, Joe @ IEC" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Macko, Joe @ IEC
Date:
Wed, 6 Sep 2006 09:31:10 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (40 lines)
Fellow techs,



Hello.

A general question came up about the need to re-bake a double sided board
after 1st side reflow/DI wash before starting 2nd side assembly. The concern
is that the board (or mounted MSDs) may absorb enough moisture going through
the high-pressure DI water in-line cleaner to potentially cause a problem
during 2nd side reflow. There are some MSDs mounted on the 1st side but both
sides are assembled before exceeding any of the component's floor life. It
has been suggested that some level of bake out should be performed after 1st
side cleaning to prevent potential problems during 2nd side reflow but the
push back is that this adds cost, handling, etc... that may introduce its
own associated problems and is not really necessary.



Thanks again. It is great to have a knowledgeable forum such as TechNet.



Joe






---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2