I agree Vladimir,
We have been using ENIG for a number of years without any "Black Pad" issues.
Regards,
Brent
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Friday, May 12, 2006 11:21 AM
To: [log in to unmask]
Subject: Re: [TN] Question about ENIG in SnPb process . . . .
I wish we stopped "scarring" people off with "Black Pad" thing. I'm yet to be convinced it's a problem NOW and I don't believe I'm alone.
Regards,
Vladimir
Vladimir Igoshev, Ph.D.
Manager, Metallurgical Lab
451 Phillip St.
Waterloo, ON N2L 3X2
Voice: (+1) 519 888-7465 x 5283
Cell: (+1) 519 572-9261
Fax: (+1) 519 888-6751
Email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: May 12, 2006 10:29 AM
To: [log in to unmask]
Subject: Re: [TN] Question about ENIG in SnPb process . . . .
Gerard
Werner has offered some advice that we all should use to our advantage; go to Google and and search for "black pad". For a PCB defect to have its own web page reaches the stratosphere of notoriety.
Staying within the manufacture's processing window will usually produce acceptable product; unfortunately small excursions beyond this window usually results in soldering problems, black pad or black pad like issues.
Unfortunately, judging by the notoriety of ENIG this occurs far too often.
Writing specs does not in itself create a robust process.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Gerard O'Brien" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 12, 2006 8:30 AM
Subject: Re: [TN] Question about ENIG in SnPb process . . . .
Camille - first of all, refer to IPC4552 which is the ENIG spec, purchase boards from suppliers following this spec and you shall have no issues.
Please be aware that reflow temperatures need to be increased slightly, 220C minimum to ensure a good solder joint formation, due to the relatively slower wetting of nickel.
Werner - please, enough with the black pad already, the world is using ENIG somewhere between 7 to 10% as the surface of choice. The old adage of you get what you pay for applies as does buyer beware - if you buy from a schlock house you will have not only solderability issues but other less obvious defects as well.
Regards
Gerard O'Brien
Photocircuits Corporation
Co-chair 4-14 plating committee.
-----Original Message-----
From: Camille Good [mailto:[log in to unmask]]
Sent: Thursday, May 11, 2006 7:28 PM
To: [log in to unmask]
Subject: [TN] Question about ENIG in SnPb process . . . .
Has anyone run into problems using PCBs with ENIG finish in regular SnPb IR reflow or wave solder processes?
I just talked to someone who said that there were industry advisories out from a couple of companies (maybe Intel & Radisys??) advising against that mixture of solder & surface finish, but I have not heard anything about that on either the TechNet or Lead-Free discussion groups, and a Google search for "SnPb solder ENIG finish" didn't turn up any immediate warnings either.
Many thanks in advance for any information,
-Camille Good
Portland, Oreong
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Messenger with Voice. Make PC-to-Phone Calls to the US (and 30+
countries) for 2¢/min or less.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
****************************************************************
The information transmitted in this message is confidential and may be privileged. Any review, retransmission, dissemination, or other use of this information by persons or entities other than the intended recipient is prohibited. If you are not the intended recipient, please notify Analogic Corporation immediately - by replying to this message or by sending an email to [log in to unmask] - and destroy all copies of this information, including any attachments, without reading or disclosing them.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest