Guenter, could you explain how the tin whisker problem is about to be
solved?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Guenter Grossmann [SMTP:[log in to unmask]]
Sent: Thursday, January 22, 2004 11:14 AM
To: [log in to unmask]
Subject: [TN] Antw: [TN] Lead-free Component Finishes
James
1) BGA's SnAgCu
Passive : Sn looks like the candidate specially since the whisker
problem seems to be about to be solved
IC's: Sn or PaAu
2) BGA's: You can solder SnAgCu balls with SnPb. However, one can
observe Pb contamination along the grain boundaries. Dave Surarski
reported early failures due to that. I couldn't say jet. We are
testing.
All the other components can be soldered with SnPb without a
problem.
3) Military is excluded of RoHS (at the moment). What do you mean
with
commercial? Look for the RoHS in the web. I don't know the address
but
Google finds it easy if you look for RoHS.
Best regards
Guenter
EMPA
Swiss Federal Laboratories for Materials Testing and Research
Centre for Reliability
Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1 823 4054
mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|