TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 11 Feb 2009 15:20:36 -0500
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gervascio, Thomas L" <[log in to unmask]>
Content-type:
text/plain; charset=us-ascii
Subject:
From:
"Gervascio, Thomas L" <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (34 lines)
I am dealing with an intermittent solder bridging on a BGA package-
about 5 percent of the time.  One avenue to make the process more robust
I was looking at was redesigning the stencil aperture.  I am currently
using a 33 mil square solder aperture giving a paste volume of 2722
cubic mils (with a 5 mil stencil). This reduced the incidence of
bridging - the previous stencil was 6 mils thick and had a print volume
of 3267 cubic mils. The ratio of the stencil aperture to the stencil
aperture area is 92%

The sphere diameter on the package is 24 mils and the pitch is  and in
the past I have made stencil apertures 2 mil larger than the maximum
diameter- in this case the volume would be 1540 cubic mils.  The ratio
of the stencil aperture wall to the stencil print area for a round
aperture is 52%. I spoke with the supplier of the component but they had
no recommendations and a cursory Google search provided no additional
information so I thought I ask the Technet folks.

Thanks


 Tom



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2