TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 16 Feb 2009 15:54:28 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner engelmaier <[log in to unmask]>
Subject:
From:
Werner engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (153 lines)
 No Tom,
SAC305 is 95.5Sn/3.0Ag/0.5Cu and SN100C is 99.2Sn/0.7Cu/0.05Ni+Ge—so there is a much higher comunality between SAC305 andSN100C than either of these two and SnPb.

Werner





 



 

-----Original Message-----
From: Tom Burek <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, 16 Feb 2009 2:53 pm
Subject: Re: [TN] Lead Free solder compatibility










Thank you for your response.  Is it a much different situation if the mix 
was SN100C and SnPb?  Also, is it not true that SN100C is most similar to 
standard the standard SnPb HASL finish that the SAC finish?
Thank you again.


Tom Burek, CID+




Werner engelmaier <[log in to unmask]> 
02/16/2009 12:34 PM

To
[log in to unmask], [log in to unmask]
cc

Subject
Re: [TN] Lead Free solder compatibility






Hi Tom,
The reliability of SAC 305 is understood; the data for SN100C are scarce.
You are creating some mish-mush alloy, but they are all in the same family 
with the same Solidus and roughly the some Liquidus. So you are not 
getting the same situation you get when you mix SnPb and SAC.

Werner


-----Original Message-----
From: Tom Burek <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, 16 Feb 2009 1:28 pm
Subject: [TN] Lead Free solder compatibility

Hello technetters,

I have a lead free solder question.  If I have a PCB with a SN100C finish 

and hand solder a component using  a tin Silver solder (SN96.5AG03 Cu.5), 

is there a possibility of creating a joint that may be l
ess reliable, 

perhaps more brittle?



Thank you





Tom Burek, CID+



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
------------
-----------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2