Mary Jane,
ANSI/IPC-SM-817 is still used as a reference for the adhesives used to bond
surface mount components to the board during the assembly and soldering
operation.
J-STD-001CS covers the basic requirements for adhesive bonding of components
for protection against vibration and shock. This is a Space Applications
document, so the bonding requirements may be more (or less) rigorous than
your application requires. Keep in mind that adhesive bonding (staking) is
application specific - what worked in the last design might make things
worse in the next design. J-STD-001CS is available as a free download from
the IPC website.
IPC-CC-830B has some useful information about the various materials that can
be used for adhesive bonding, even though it is primarily for conformal
coatings.
IPC-2221A has some additional info.
Regards,
Bob
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mary Jane Chism
Sent: Tuesday, May 31, 2005 3:40 PM
To: [log in to unmask]
Subject: [TN] Staking Adhesive
Other than the IPC-A-610 document, is there an IPC document that gives
specifications on staking adhesive?
Thanks.
Mary Jane Chism
Kimball Electronics
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|