TECHNET Archives

September 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 4 Sep 2014 19:54:41 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jim West <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jim West <[log in to unmask]>
Parts/Attachments:
text/plain (15 lines)
Our paste printers are having difficulty recognizing the fiducials on an older board that has been running for years.  The board house is applying HASL and because of that, as most are aware, the solder covering the fiducial pad will be inconsistent.  I'm told that this has been an ongoing issue and the problem comes and goes.
We have three printers that are older that do not allow us to adjust the lighting.

I can't remember if we can have the board house apply HASL on just the component pads and not the fiducials?  Any other suggestions?

Thanks,
Jim



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2