Ralph,
Of the different tests available, I would suggest ion chromatography per
IPC-TM-650, method 2.3.28. You get more meaningful data than any of the
other available tests.
Doug Pauls
"Taylor, Ralph W"
<ralph.w.taylor@L To: [log in to unmask]
MCO.COM> cc:
Sent by: TechNet Subject: [TN] Aluminum Wire bond COB PWB cleanliness
<[log in to unmask]>
08/29/2003 07:38
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Taylor, Ralph W"
Any recommendations for cleanliness testing for acceptance of gold plated
PWB's intended for Chip On Board applications using aluminum wire wire
bonding?
Ralph W. Taylor
Lockheed Martin Maritime Systems & Sensors
Moorestown N.J.
Tele: 856-722-2639 Fax: 856-722-4410
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|