TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Mon, 19 Mar 2001 11:50:34 +0800
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (74 lines)
Hi, Don,

I take it you're building either a mixed technology board, and/or are CR
soldering an SMT board followed by wave sodlering edge connectors. As
Werner says, as long as you achieve full melting point again, there should
be no problem, though with a no-clean process I might be concerned about
the lack of fluxing left to maintain good wetting. If you don't get
adequate wetting, you may get very course crystaline joints and de-wetting.

Is hand soldering a viable alternative to wave soldering, or are there too
many joints?

Regards

Pete Duncan
Asst Principal Engineer
ST Aerospace




Werner Engelmaier <[log in to unmask]>@IPC.ORG> on 03/17/2001 04:41:53 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to [log in to unmask]

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:
Subject:  Re: [TN]




Hi Donn,
As long as the SJs completely liquefy in the second soldering process, no
reliability down-side exists--it is like a second reflow. I am not clear
why
you want to do this however.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2