TECHNET Archives

June 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Louis Hart <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Louis Hart <[log in to unmask]>
Date:
Tue, 11 Jun 2013 16:17:13 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (51 lines)
They are expressions of incompetence and cowardice. They guy doesn't know what he is doing and does not even have the nerve to admit it. Louis Hart 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Tuesday, June 11, 2013 9:29 AM
To: [log in to unmask]
Subject: Re: [TN] Dewetting on high current connector

It's a very common statement!   So common, that we are no longer get SHOCK when we hear it.   It's an acceptance of poor quality.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Tuesday, June 11, 2013 8:17 AM
To: [log in to unmask]
Subject: Re: [TN] Dewetting on high current connector

Yes, indeed!

How many times have we heard those very same words from vendors all over?

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Tuesday, June 11, 2013 9:02 AM
To: [log in to unmask]
Subject: Re: [TN] Dewetting on high current connector

I feel an indication of a sarcasm?




On 11 June 2013 11:35, Mike Fenner <[log in to unmask]> wrote:

> Yes, but first they have to say:
>
> Don't understand this we're not doing anything different No one else 
> has complained This is the first time we ever had this.
>
>
> Mike
>
> 
_____________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2